SKU
10120012092
Thermanit Nicro 82 2.4x1000mm
Böhler 82824 (5kg)
- Stainless; heat and high temperature resistant.
Read more
- Good toughness at subzero temperatures as low as –269 °C (–452 °F). - Good for welding austenitic-ferritic joints. - No Cr carbide zone that becomes brittle in the ferrite weld deposit transition zone, even as a result of heat treatments above 300 °C (572 °F). - Good for fabricating tough joints and surfacing with heat resistant Cr- and CrNi- steels and Ni-alloys. - Temperature limits: 900 °C max. (1652 °F) for fully stressed welds. Resistant to scaling up to 1000 °C (1832 °F). - Yield strength: 400 MPa - Tensile strength: 620 MPa - Elongation: 35 % |