Customer number attached to your company account has been blocked. If you have any questions, please contact your company admin user or [email protected].
10120014834

Thermanit 30/40 E 2.4x1000mm

Böhler 68626 (5kg)
kg

Store availability is shown for logged in users. Product availability subject to prior sales.

Description

  • At central warehouse in Finland(delivery in 3-4 days)
  • In Megacenter (see store availability)
  • Ordered upon request or limited availability, delivery time will be confirmed after order


The prices are shown to registered users excluding VAT (VAT 0%)

Details
- Nickel based alloy; resistant to intercrystalline corrosion and wet corrosion up to 450 °C (842 °F).
- Good corrosion resistance, especially in reducing environment.
- For joining and surfacing work with matching and similar – non-stabilized and stabilized – fully austenitic steels/cast steel grades containing Mo (and Cu).
- For joining mentioned steels with unalloyed/low-alloy steels.
- Yield strength: 350 MPa
- Tensile strength: 550 MPa
- Elongation: 30 %